Study on the Process of Sinking Copper and Arsenic with Iron Powder in Low Copper Reduction Leaching Solution
CSTR:
Author:
Affiliation:

Yunxi Wenshan Zinc & Indium Smelting Co., Ltd, Wenshan 663701 ,China

Clc Number:

TF813;TF803

Fund Project:

  • Article
  • |
  • Figures
  • |
  • Metrics
  • |
  • Reference
  • |
  • Related
  • |
  • Cited by
  • |
  • Materials
  • |
  • Comments
    Abstract:

    In this paper, the low copper reduction leaching solution with copper content of 0.52g/L was used as raw material, and iron powder was used to carry out copper and arsenic precipitation experiments. The effects of iron powder coefficient, reaction time, reaction temperature and copper arsenic ratio on copper and arsenic precipitation were investigated. The results show that the addition coefficient of iron powder is the main factor affecting the effect of copper precipitation and arsenic precipitation. The ratio of copper to arsenic has a great influence on the removal of arsenic, and the reaction time and reaction temperature have little effect on the effect of copper precipitation and arsenic precipitation. When the iron powder coefficient reaches 1.8, the reaction temperature is maintained above 70℃, the reaction time is 1h, and the ratio of copper to arsenic is 2.36, the copper deposition rate and arsenic deposition rate are 82.69% and 72.73%, respectively. The copper content in the liquid after copper deposition is 0.09g/L, and the arsenic content is 0.06g/L.

    Reference
    Related
    Cited by
Get Citation

李云,陶家荣,朱应旭,等.低铜还原浸出液中铁粉沉铜沉砷工艺探索[J].绿色矿冶,2025,41(4):84-88.

Copy
Related Videos

Share
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:April 24,2025
  • Revised:
  • Adopted:
  • Online: November 13,2025
  • Published:
Article QR Code