    摘要:

    采用氢氧化钠溶液对高碳铝土矿进行预处理,使高碳铝土矿中碳酸盐浸出进入溶液相中,从而实现脱碳的目的,分别研究了氢氧化钠浓度、反应温度、反应时间、矿浆固含量对高碳铝土矿预处理脱碳效果的影响。根据试验结果,高碳铝土矿中碳主要为无机菱铁矿碳酸盐,其脱碳的较优反应条件:氢氧化钠浓度10%,反应温度60℃,反应时间80min,矿浆固含量控制800g/L。在最佳处理条件下,高碳铝土矿全碳含量可由1.34%降低至0.35%以下,无机碳脱除率可达到90%以上。预处理后碳酸钠溶液通过石灰乳苛化回收碱液,碱液返回循环使用。该方法得到的碳酸钠溶液几乎不含铝酸钠,在石灰乳苛化过程不会造成氧化铝失,有效解决了传统铝酸钠溶液体系排盐苛化无法避免氧化铝损失的难题。预处理后矿石含碳量可达到0.35%以下,满足拜耳法氧化铝生产系统控碳要求,拜耳法氧化铝生产过程不再需要排盐,节省排盐蒸汽消耗,并消除了碳酸钠对拜耳法氧化铝生产过程的影响。

    Abstract:

    The pretreatment of the high carbon bauxite was performed by Using sodium hydroxide solution,the carbonate in the high carbon bauxite was leached into the solution phase and the purpose of decarbonization was achieved. The effects of sodium hydroxide concentration, reaction temperature, reaction time and mineral slurry fixation content on the decarbonization effect of the high carbon bauxite were studied respectively. According to the test results, the carbon in high-carbon bauxite is mainly inorganic siderite carbonate,and its optimal reaction conditions for decarbonization are as follows: sodium hydroxide concentration 10%, reaction temperature 60℃, reaction time 80min, and slurry solid content control 800g/L. Under the optimal treatment conditions, the total carbon content of high-carbon ore can be reduced from 1.34% to below 0.35%, and the inorganic carbon removal rate can reach more than 90%. After pretreatment, the sodium carbonate solution was recovered by caustic reaction of lime milk, and the base solution was returned to circulation. The sodium carbonate solution obtained by this method does not contain sodium aluminate, which will not cause alumina loss in the caustic reaction process of lime milk, and effectively solves the problem of traditional sodium aluminate solution system cannot avoid alumina loss. After pretreatment, the carbon content of the ore can reach less than 0.35%, which meets the carbon control requirements of the Bayer alumina production system. The Bayer alumina production process no longer needs salt discharge, saves the consumption of salt discharge steam, and eliminates the impact of sodium carbonate on the Bayer alumina production process.

    参考文献
    相似文献
    引证文献
引用本文

曾宪飞.高碳铝土矿碱法预处理脱碳试验研究[J].绿色矿冶,2025,41(6):50-56.